INCOLOY 800 Folja tad-Dejta
1. Informazzjoni Ġenerali
Grad:Incoloy 800 (UNS N08800)
Tip:Liga tan-nikil-ħadid-kromju
Standards:ASTM B407, B409, B163, ASME SB -163, SB -409
2. Kompożizzjoni kimika (wt.%)
| Elemnt | Min | Massimu |
|---|---|---|
| Nikkil (Ni) | 30.0 | 35.0 |
| Kromju (CR) | 19.0 | 23.0 |
| Ħadid (Fe) | Bilanċ | - |
| Karbonju (Ċ) | - | 0.10 |
| Manganiż (MN) | - | 1.00 |
| Silikon (SI) | - | 1.00 |
| Titanium (TI) | 0.15 | 0.60 |
| Aluminju (AL) | 0.15 | 0.60 |
3. Propjetajiet mekkaniċi
| Proprjetà | Valur tipiku |
|---|---|
| Qawwa tat-tensjoni | 515 - 690 MPa (75-100 ksi) |
| Qawwa tar-Rendiment (0. 2%) | 205 - 310 MPa (30-45 KSI) |
| Titwil | Akbar minn jew daqs 30% |
| Ebusija (brinell) | 170 - 210 HB |
| Modulu ta 'elastiċità | ~ 200 GPA (29, 000 ksi) |
4. Propjetajiet fiżiċi
| Proprjetà | Valur |
|---|---|
| Densità | 8. 0 g \/ cm³ |
| Firxa tat-tidwib | 1370 - 1425 grad |
| Konduttività termali | ~ 11.4 w \/ m · k (100 grad) |
| Koeffiċjent ta 'espansjoni termali | 13.1 µm \/ m · Grad (20-100 grad) |
5. Limiti tat-temperatura
| Ambjent | Temperatura massima tas-servizz |
|---|---|
| Atmosferi ossidanti | Sa 1100 grad (grad 2010 F) |
| Tnaqqis jew karburizzanti | Aktar baxx, jiddependi fuq il-kundizzjonijiet |
6. Reżistenza għall-korrużjoni
Reżistenza eċċellenti għall-ossidazzjoni u l-karburizzazzjoni.
Stabbli f'ambjenti ħafifa ossidanti u jnaqqsu.
Reżistenti għall-preċipitazzjoni tal-karbur minħabba stabbilizzaturi tat-titanju u tal-aluminju.
7. Applikazzjonijiet
Skambjaturi tas-sħana
Komponenti tal-forn
Proċessar kimiku u petrokimiku
Komponenti tar-reatturi nukleari
Elementi tat-tisħin